Updated
Recycled Glass Fiber Reinforced PET-G (rPETG GF)
rPETG GF is recycled PET-G reinforced with glass fiber. Enhanced stiffness and good chemical resistance.
rPETG GF: composition and designation
| Parameter | rPETG GF |
|---|---|
| Catalog designation | Recycled Glass Fiber Reinforced PET-G (rPETG GF) |
| Base polymer | PET-G |
| Filler | Glass fiber (GF) |
| Feedstock | Recycled PET-G |
Composition and designations follow the Protype catalog. Filler percentages and Shore designations describe the filament; they are not measurements of printed parts.
Comparison: rPETG GF / PET-G / PETG GF10
| Parameter | rPETG GF | PET-G | PETG GF10 |
|---|---|---|---|
| Base polymer | PET-G | PET-G | PET-G |
| Filler | Glass fiber (GF) | Not specified in the catalog | Glass fiber (GF) (10%) |
| Maximum nozzle temperature | 250°C | 250°C | 250°C |
| Bed Temperature | 70–80°C | 70–80°C | 70–80°C |
| Chamber Temperature | not required | not required | not required |
| Print Speed | 40–60 mm/s | 50–80 mm/s | 40–60 mm/s |
| Cooling Fan | 20–40% | 30–50% | 20–40% |
| Drying: temperature / minimum time | 55°C / 3 h | 50°C / 2 h | 55°C / 2 h |
Printing and drying settings come from the Protype catalog, which lists them for REC materials. Check the manufacturer datasheet for the specific grade: these values are not a qualified print profile or a measure of part heat resistance.
Manufacturer's Print Settings
| Maximum nozzle temperature | 250°C |
| Bed Temperature | 70–80°C |
| Chamber Temperature | not required |
| Print Speed | 40–60 mm/s |
| Cooling Fan | 20–40% |
Drying Parameters
Recommendation
The catalog lists 55 °C and at least 3 h of drying for rPETG GF.
⚠ Settings depend on the filament grade. Before drying, check the manufacturer datasheet and the spool temperature limit.
Applications
Printer Compatibility
Trusted Manufacturers
REC is a Russian manufacturer of engineering filaments. We check its materials by printing and keep profiles for them.